INTEFIX FAST
Chemical Anchorage

|
DESCRIPTION |
Made up of system resins polyester bimembers whose polymerization happens by means of the mixing of the members. It comes automatically activated to every injection thanks to a particular small beak of external mix for use it also in successive times. |
|
PROPRIETIES |
Easy and fast to employ it. Thanks to its high value of adhesion and its ability to penetrate in the porosity and the hollow zones, concur a sure implantation on whichever support: full and empty masonry, natural cliff and stones, concrete, armed concrete and wood. |
|
APPLICATIONS |
Indicated for slab implantations, metallic carpentries, enclosure, lockings, cancel, bars and irons of armor etc. It console to be employed also like mass of ideal repair and filling. it fits for difficult implantations in the restructures, the reorganizations and the cases in which it is not possible to use a mechanical dowel. Natural Cls, Stones, Mattoni, Armed Concrete: The advantages in using Intefix Fast come exalted in presence of these materials in how much obtain remarkable permissible cargos varying, to second of the requirements, the element to fix and the depth of the anchorage. In presence of old walls structures of uncertain consistency and uniformity, the resin penetrates in empty adjacent the practiced hole, forming an only body with the structure and offering therefore emergency of estate. Materials Pierced Buildings: It comes finally resolved the problem of the sure implantation on empty masonry. The injection of the resin in the appropriate net compass, provokes the spillage of this last one in the zones of empty. It guarantees a reliable and economic implantation. |
|
HOW TO USE |
Full Materials: To practice to a hole of diameter and appropriate depths like from indispensable Tab 1 It needfor a good result to accurately clean up the residual holes from of powder or water. Before placing the cartridge in the gun to unscrew the threaded stopper external, to remove the stopper to internal pressure, to screw the mixer. For the cartridges from 380 mm to remove the protection cover on the inferior part. For the cartridges from 150 mm to put the appropriate piston in the back. To put the cartridge in the appropriate gun. In order to guarantee the just mix between the two members to make the product out until the appearance of one uniform coloration. inject the resin beginning from the bottom of the hole and fill until to 2/3 of its volume. To insert the bar threaded turn it to improve the adhesion. Before applying the cargo to observe the times indicated in Tab 3. Pierced Materials: To gain a hole of dimensions like from Tab 2. To insert the net compass in order to concur to dose the resin and to center the bar. To proceed like for the full materials. |
|
Setting times |
The times of polymerization vary with the temperature. E' important to respect the times minimums between it puts down and the application of the brought back cargo like in Tab 3. |
Tab 1 compact Materials
|
Diam. bar milimeter |
Diam hole milimeter |
Prof hole milimeter |
|
8 |
10 |
80 |
|
10 |
12 |
90 |
|
12 |
14 |
110 |
|
16 |
18 |
125 |
|
20 |
24 |
170 |
|
24 |
28 |
210 |
Tab2 Material Pierced
Tab3 Times of consolidation
|
Cargo values |
The cargo limits for natural stones, lateritious pierced floods are tax from the mechanical characteristics of the supports (in all the traction tests observe always the breach of the support). On the concrete of class RCK > 250Kg/cm, mechanically more resistant, it prevails in the tests of traction, the breach of the threaded metallic hinge. In all the laboratory tests the breaking strength exceeds on concrete with threaded bar diam.8 mm the 1500 Kg: it is advisable to apply an equal reserve factor to 4. For high or however advanced cargo values to 1500Kg it is recommended to use hinges of diameter adapted with accredited characteristics and to verify on the place the estate abilities. |
|
Measures of Emergency |
To use protection for face, hands, eyes. In case of contact with the skin, wash endured with water and soap. In case of contact with the eyes, wash abundantly with water and call a doctor. Annoying and inflammable product |
|
Stoccaggio |
If it comes conserved in fresh place and dry(< 25°), in pack sluices, the time of storage will be of 12 months from the production date. If the cartridge does not come completely emptied, to hold inserted the mixer therefore from being able to re-use the product in successive times (max 1 month).To re-use enough to replace the mixer. |
|
Confection |
Cartridges from 150 mm Cartridges from 380 mm |